OUR LABORATORY
 
 
 
 
 
 
 
 
 
 
Tests
Average Test Results
  Crazing Test Completely Craze Proof  
  Water Absorption Less Than 0.5 %  
  Modulus Of Rupture More Than 625 Kg/Sq. Cm  
  Chemical Resistance HIghly Resistant  
  Resistance To Staining And Burning Stain And Burn Proof  
 